acsr material
Pure aluminum has a density of 2.7 g/cm3, ? her 1.4. 10-5, melting point 6580C and not corrosive. Conductivity of aluminum by 35 m/ohm.mm2 or roughly 61, 4% conductivity copper. Be formed because of soft pure aluminum, the tensile strength only 9 kg/mm2. For that if aluminum is used as the Conductor of dimensions large enough, always.
reinforced with steel or aluminum alloy. The use of such ex alnya on: ACSR (Aluminium Conductor Steel Reinforced), pickles (Aluminium Conductor Alloy Reinforced). Conductor construction of aluminum and steel.
Another is the use of aluminum for the busbar, and because of certain reasons such as economic, then made conductive insulated aluminum, such as: ACSR - OW. According to the ASA (American Standards Association).
ACSR and ACAR
Tagging 1045 for aluminum forgings, means:
1xxx shows 99% purity, x0xx no examination of the residual contamination of 1% - 0.45% = 55 %, xx45 showed 99.45% of the aluminum material.